Factory direct from Jingdezhen · Wholesale, OEM and retail

How We Control Quality, Kiln to Carton

Every piece is coded back to its kiln run and shift. In 2025 that system kept our complaint rate at 0.07% and transit breakage at 0.21%.

Photo

Min Zhou, Quality Director (17 years)

Three inspection stages

StageWhat we checkLimit
IncomingClay moisture and plasticity, iron and impurities, plaster mold size18–20% moisture; molds ±0.3 mm
In processSize, wall, seams, glaze thickness, decal position, recorded every 2 hoursWall ±0.4 mm; glaze 0.25–0.35 mm
FinalMachine vision plus a manual check on every piece: size, colour, lead and cadmiumDefect standard below

Manual and machine vision inspection

Inspector checking a porcelain plate against the light
Manual inspection
Machine vision station inspecting porcelain bowls on a conveyor
Machine vision

Our defect standard

ItemAccepted
PinholesUp to 2 per piece, 0.5 mm or less, never on a food-contact surface
Specks1 per piece, 0.8 mm or less
Orange peelNot visible at 30 cm under 500 lux
ColourΔE 1.5 within a batch, 2.0 between batches
WarpOvality 1.5% or less; plates warp 1.2 mm or less
Rim size±1.5 mm
Weight±3%
Gold lineContinuous with no gaps; survives 50 rubs

Our lab

A 320 m² lab with an Agilent 7900 ICP-MS for lead and cadmium, an X-Rite Ci7800 spectrophotometer, and thermal shock and impact rigs. We hold lead and cadmium to half the legal limit.

Lab technician running lead and cadmium tests on an ICP-MS

Final inspection and claims

Final sampling is AQL 2.5 (major) and 4.0 (minor) by default, or 1.5 if you ask. Your own inspector is welcome. Raise a quality claim within 30 days of arrival and we send a draft 8D report within 48 hours. Our liability covers up to the full order value, backed by USD 2 million of product liability insurance.

FAQ

Our tested lines are tested to FDA CPG 7117.06/07 and ASTM C738 (SGS-CSTC-2026-QZ-04187), LFGB and EU 1935/2004 (LFGB-20260305-118), California Prop 65, Canada SOR/2016-175 and Japan Notice 370. Ask us which reports cover the models you order.

41 SKUs are tested microwave safe (700 W, 5 min, 20 cycles) and 9 hotel shapes for 1,000 commercial dishwasher cycles. Pieces with gold lines are not microwave safe.

Tell us within 30 days of arrival with photos. We reply with an 8D draft within 48 hours and replace or credit the loss.

AQL 2.5 by default, 1.5 on request; major defects 2.5, minor 4.0.

On our own Agilent 7900 ICP-MS to FDA and LFGB methods, with an internal limit at half the legal limit.

Yes. Book 3 working days ahead and they can come at any time.

Raise it within 30 days; we send a first 8D report within 48 hours, with liability up to the full order value.

We keep a sample of every incoming clay batch, and for N-01 we keep a sample of every production batch for three years.

Batches of food-contact pieces are checked on our ICP-MS against an internal limit of half the legal limit.

0.07% in our 2025 records, with transit breakage of 0.21%.

Certificates and test reports

ISO 9001:2015 Quality management, TONFO (Jiangxi Tuofeng Ceramics Group)
ISO 9001:2015 Quality Management System
Lead and cadmium release, FDA / ASTM C738 · No. T52210320163TC
Lead and cadmium release, FDA / ASTM C738 · No. T52210320163TC
Thermal shock and handle strength · No. GZHG1405016068CW
Thermal shock and handle strength · No. GZHG1405016068CW
Dishwasher resistance, EN 12875 · No. AGC05443230702-001
Dishwasher resistance, EN 12875 · No. AGC05443230702-001
LFGB food contact (TÜV Rheinland) · No. 0003287451/30 AZ 337537
LFGB food contact (TÜV Rheinland) · No. 0003287451/30 AZ 337537
California Proposition 65, lead and cadmium · No. CANHL24019243501
California Proposition 65, lead and cadmium · No. CANHL24019243501
Canada SOR/2016-175, lead and cadmium · No. 23W-016190
Canada SOR/2016-175, lead and cadmium · No. 23W-016190
Japan Food Sanitation Law · No. HKGH02630796
Japan Food Sanitation Law · No. HKGH02630796

Copies of certificates and test reports are shared with buyers on request.

In the test lab

Technician placing a glaze sample in a spectrophotometer
Glaze colour measurement
Thermal shock test baths with baskets of porcelain cups
Thermal shock test
Drop test rig holding a shipping carton above the floor
Carton drop test

Three levels of inspection

StageWhat is checkedLimitRecord
Incoming (IQC)Clay moisture and plasticity, iron and impurities, plaster mold size and surfaceMoisture 18–20%; mold ±0.3 mmSample kept per batch
In process (IPQC)Formed size, wall thickness, seams, glaze thickness, decal positionWall ±0.4 mm; glaze 0.25–0.35 mmLogged every 2 hours
Final (FQA)Machine vision plus 100% manual check; size, colour, lead and cadmium releaseOur defect standard belowTraced to kiln run and team

Defect limits, item by item

This is the standard every piece is sorted against before packing.

DefectAccept only if
Pinholes≤0.5 mm across, no more than 2 per piece, and not on a food-contact surface
Kiln grit≤0.8 mm across, no more than 1 per piece
Orange peelNot obvious at 30 cm under 500 lux
ColourΔE ≤1.5 within a batch, ≤2.0 between batches
WarpRim ovality ≤1.5%; plates warp ≤1.2 mm
Rim size±1.5 mm
Lead and cadmiumInternal limit at 50% of the legal limit
Gold lineContinuous, no gaps or burrs; 50 rubs without wearing through

Our test lab

EquipmentUsed for
ICP-MS (Agilent 7900)Lead and cadmium release to FDA and LFGB methods
Spectrophotometer (X-Rite Ci7800)Colour difference ΔE at D65/10°
Thermal shock rig180 °C to 20 °C quench, ASTM C554
Ball impact tester100 g steel ball dropped from 1 m
Bending testerThree-point bend, 0–5 kN
Whiteness and absorptionWhiteness meter, vacuum water-absorption rig
Microwave and dishwasher700 W microwave; EN 12875 dishwasher, 1,000 cycles
Climate chamberAgeing at 40 °C / 90% RH

Our lab is 320 m² and sits inside the factory, so a batch can be tested before it is packed.

Results

In our records, transit breakage runs at 0.21%, the customer complaint rate at 0.07% and on-time delivery at 96.8%. N-01, a Nordic home retail group, has bought from us since 2018 without a major quality incident.

PropertyOur standard
Water absorption≤0.5% (high-white porcelain ≤0.3%)
Whiteness≥78
Bending strengthStrengthened porcelain ≥120 MPa
Glaze hardness≥6 Mohs
Thermal shock180 °C to 20 °C water quench, no cracks (ASTM C554)
Lead and cadmium releaseInternal limit at 50% of the legal limit
ColourΔE ≤1.5 within a batch, ≤2.0 between batches (X-Rite Ci7800, D65/10°)
Rim diameter±1.5 mm; ovality ≤1.5%
Piece weight±3%
DishwasherEN 12875-1 / EN 12875-5, 1,000 cycles
Microwave700 W, 5 minutes, 20 cycles
Carton drop1.2 m, six faces, three edges, one corner (ISTA 1A / 3A)

How a piece is made, and checked

StepWhat we control
1 ClayKaolin, feldspar and quartz ball-milled for 18 hours, vacuum-pugged twice, moisture 18–20%
2 FormingRoller forming, slip casting or isostatic pressing; wall thickness ±0.4 mm
3 Trimming and bisqueBisque fired at 800–900 °C to burn out water and organic matter
4 GlazingDip, spray or pour; glaze 0.25–0.35 mm thick, robot repeatability ±0.02 mm
5 DecorationUnderglaze, in-glaze, decal, gold line, laser marking; food-contact surfaces use underglaze or in-glaze only
6 Firing1,260–1,320 °C, ±8 °C across the kiln, 9 thermocouples logged
7 Sorting and packingMachine vision plus a 100% manual check, AQL 2.5 audit, every carton coded

Reports we hold

ReportLabStandardCoversValid to
SGS-CSTC-2026-QZ-04187SGS-CSTCFDA CPG 7117.06/07, ASTM C738, ASTM C92714 series, 62 SKUs15 Apr 2027
SGS-CSTC-2026-QZ-05233SGS-CSTCASTM C554 thermal shock; microwave 700 W × 5 min × 2041 microwave-safe SKUs7 May 2027
SGS-CSTC-2026-QZ-05310SGS-CSTCEN 12875-1 / -5, 1,000 cycles9 hotel shapes14 May 2027
LFGB-20260305-118TÜV RheinlandLFGB §30/31, (EC) No 1935/2004All food-contact shapes4 Mar 2027
EU-DOC-TF-2026-007TONFO (manufacturer's declaration)(EC) No 1935/2004 Article 16All categories, issued with each batch11 Mar 2027
SGS-CSTC-2026-QZ-06114SGS-CSTCCalifornia Proposition 65 (lead, cadmium)38 US-line SKUs1 Jun 2027
SGS-CSTC-2026-QZ-06115SGS-CSTCCanada SOR/2016-17538 Canada-line SKUs1 Jun 2027
JFRL-2026-0418-TFJapan Food Research LaboratoriesFood Sanitation Act, MHLW Notice No. 37022 Japan-line SKUs17 Apr 2027

Reports travel with the container, so you can clear customs and list the goods with them.

Inspection, claims and response times

You or a third party can inspect before loading. If something is wrong on arrival, claims are accepted for 30 days.

StageOur time
First replyWithin 24 hours on working days
Formal quotationWithin 48 hours
SamplesSent 7–15 days after approval
Order confirmationWithin 2 working days of the deposit
Progress reportsPhotos every 10 days
InspectionBook 3 working days ahead
LoadingWithin 5 days of a passed inspection
DocumentsSent within 3 working days of sailing
Quality claimsAccepted up to 30 days after arrival, first 8D in 48 hours

Audits that check our quality system

  • ISO 9001:2015, certificate 00224Q22327R0M, issued by CQM.
  • Two measurement management systems rated AAA, from CQM and the CAQ Quality Assurance Centre.
  • Retailer audits: Walmart FCCA (green), IKEA IWAY 6.0, Target, Costco and Disney ILS.
  • Social compliance: amfori BSCI Grade B and Sedex SMETA 4-Pillar.

What each test tells you

Lead and cadmium release (FDA CPG 7117.06/07, ASTM C738, ASTM C927). A weak acid is left in the piece for 24 hours and the liquid is analysed for lead and cadmium. ASTM C927 tests the outer lip and rim of drinking vessels, where a mouth touches decoration. FDA sets the limits; we hold every food-contact shape to half of them.

LFGB and (EC) No 1935/2004. Germany's food and feed code and the EU framework for materials in contact with food. Retailers in the EU ask for the test report and the manufacturer's declaration of conformity; we issue the declaration with each batch.

California Proposition 65. Requires a warning on products that expose users to listed chemicals, including lead and cadmium, above set levels. Our report gives lead and cadmium results for 38 US-line SKUs, which retailers use to decide on labelling.

Canada SOR/2016-175 and Japan Notice No. 370. Each country's own limits for lead and cadmium from glazed ceramics. Our reports cover 38 Canada-line and 22 Japan-line SKUs.

Thermal shock (ASTM C554). The piece is heated and dropped into cold water; we use 180 °C into 20 °C. It shows whether a mug can take boiling water or a plate can go from oven to sink without cracking.

Dishwasher (EN 12875-1 / -5). Repeated commercial wash cycles, then a check for glaze wear and fading. Our hotel shapes pass 1,000 cycles.

Microwave. 700 W for 5 minutes, 20 times, checking for heating, cracking and sparking. Anything with gold or metal decoration fails by design and is never sold as microwave safe.

Colour (ΔE). A number for how far a colour is from the reference. Below about 1.5 most people cannot see a difference side by side; we hold ΔE 1.5 within a batch and 2.0 between batches.

Which of these tests your market requires, and how to read the report, is covered in how food-contact rules differ by market.

How AQL inspection works

AQL (acceptable quality limit) sets how many pieces an inspector draws from a lot and how many defects are allowed before the lot fails. At AQL 2.5 for major defects and 4.0 for minor, a larger lot means a larger sample, but the pass mark stays the same proportion.

Major defects are those a customer would return the piece for: cracks, chips, pinholes on a food surface, wrong colour. Minor defects are visible but do not stop the piece being used, such as a small glaze speck on the base.

We sort every piece by machine vision and by hand before packing, then audit at AQL 2.5. If you want a stricter level, we inspect to AQL 1.5. Your own inspector or a third party can sample the goods before loading if booked 3 working days ahead.

What happens to a piece that fails

A piece rejected at sorting does not go into stock. Tunnel kiln 4# handles second glaze firings, so some glaze faults can be refired; rejects are traced to the kiln run and team so the cause can be found.

Because each tunnel kiln has 9 thermocouples logging to the MES, a colour or firing problem can be traced to the kiln run and the firing curve.

How we hold colour from order to reorder

Colour drifts for three reasons: a change in raw material, a change in glaze thickness and a change in firing. We control all three. Clay is checked on arrival for moisture, plasticity and iron, and a sample of each batch is kept. Glaze is applied by robots to 0.25–0.35 mm, repeating to ±0.02 mm. Firing curves are logged for every kiln run.

Every batch is measured on an X-Rite Ci7800 spectrophotometer under D65 light and held to ΔE 1.5 within the batch and 2.0 between batches. For customers who need an exact match over years, such as D-01, we keep a glaze recipe for them alone.

Who leads quality

Our quality director has 17 years in ceramics and has led our BSCI, SMETA and FCCA audits. The quality team is 32 people across incoming inspection, in-process checks, final sorting and the lab, out of 268 staff.

Reading our reports

Each report lists the lab, the standard, the date and the SKUs covered. When you buy, check that your models are on the report and that the report covers your market: FDA and ASTM for the US, LFGB for Germany and the EU, SOR/2016-175 for Canada, Notice No. 370 for Japan.

Reports are valid for a year from issue; ours run to 2027. If your decoration is new, ask whether it needs its own test before shipping.

Common porcelain defects, explained

Pinholes are tiny holes in the glaze left by gas escaping during firing. On a food surface they can trap dirt, so we reject any on a food-contact surface and allow no more than 2 elsewhere.

Kiln grit is a speck of refractory or dust fused into the glaze. We allow one, no larger than 0.8 mm.

Orange peel is a dimpled glaze surface. We judge it at 30 cm under 500 lux; if it is obvious, the piece fails.

Warp is a plate that does not sit flat or a rim that is not round. Plates may warp no more than 1.2 mm and rims may be no more than 1.5% oval.

Crazing is a network of fine cracks in the glaze, caused when glaze and body shrink at different rates. Our thermal shock test, 180 °C into 20 °C water, is designed to show it.

Inspection booking and what your inspector sees

Your inspector or a third-party firm can visit any working day; book 3 working days ahead. They draw cartons at random from the finished lot, open them, check pieces against the approved sample and our defect standard, and measure size, weight and colour.

If the lot passes, loading follows within 5 days.

Food safety, step by step

Food safety in porcelain comes down to what can leave the glaze and enter food. Lead and cadmium can come from glaze or decoration pigments, so control starts with materials: our underglaze process, invention patent ZL 2023 1 0822016.8, was developed for low lead and cadmium release.

Second, decoration is kept off food-contact surfaces: underglaze and in-glaze only where food or a mouth touches, decals and gold lines on the outside.

Third, firing: glaze that is not fully fired can release more metal, so each tunnel kiln's curve is logged and the temperature is held within ±8 °C across the kiln.

Fourth, testing: batches are checked on our own ICP-MS against an internal limit of half the legal limit, and third-party reports from SGS-CSTC, TÜV Rheinland and JFRL cover each market.

When to ask for a stricter check

AQL 2.5 suits most retail and wholesale orders. Ask for AQL 1.5 if the pieces go into gift boxes, carry a brand that will be judged up close, or are new to your range. For colour-critical programmes, ask us to keep batch samples, as we do for N-01, whose samples we keep for three years.

If a claim does arise, our first 8D report within 48 hours sets out the cause and the correction, and our liability runs up to the full order value.

Quality figures

Our 2025 records show transit breakage of 0.21%, a customer complaint rate of 0.07% and on-time delivery of 96.8%, across 17.8 million pieces delivered and 620 export containers.

Who checks your goods

32 of our 268 people work in quality: incoming inspection, in-process checks every 2 hours, final sorting and the lab. Our quality director has 17 years in ceramics, and every piece that leaves is traced to its kiln run and team, so a question about one carton can be answered from the records, not from memory.

Order terms in brief

The minimums that set how large a batch, and so an inspection sample, will be.

TopicWhat applies hereFull details
Minimums and lead timesStandard model on an existing mold: 500 pcs, 25–30 days; New mold: 3,000 pcs, 45–55 days.Shipping and trade terms

Tell us what you need

A product, a quantity and a market are enough to start. We reply within 24 working hours.